Description: • Vary the concentration of MeTPA spin and measure contact angle
• Goal is to find a range of concentrations wide enough to produce meaningful variations in contact angle, to do subsequent efficiency and stability studies in devices on
The following samples are staged for launch. Launch the experiment.
| Group | Path | Substrate Type | Sample ID |
|---|---|---|---|
|
Group "Anneal only"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG1 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG2 | ||
|
Group "EtOH only"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG3 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG4 | ||
|
Group "0.01 mg/mL"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG5 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG6 | ||
|
Group "0.025 mg/mL"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG9 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG10 | ||
|
Group "0.05 mg/mL"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG11 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG12 | ||
|
Group "0.1 mg/mL"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG13 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG14 | ||
|
Group "0.5 mg/mL"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG7 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG8 | ||
|
Group "0.5 mg/mL NoAnneal"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG15 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG16 | ||
|
Group "Control"
|
ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG17 | |
| ColoCon ITO standard (20ohm/cm2) (CCC0068) | 250409SG18 |